Aggregate buying guides

Understanding Aggregate Gradation

Read an illustrative gradation curve and its sieve table. Practice percent-passing calculations and learn what to compare with the project’s grading limits.

Conceptual comparison of coarse, intermediate, and fine aggregate particle sizes; actual grading depends on the product.

Gradation is the distribution of particle sizes in aggregate. Two products with the same largest stone can contain different amounts of smaller particles and fines. Use the sieve results to compare the full distribution with your project’s grading limits.

What the report is telling you

Report termMeaningBuyer check
Sieve openingThe opening used to separate particle sizes.Confirm the units and sieve designation.
Percent passingThe cumulative proportion by mass that passes a stated sieve.Read the sequence, not one result in isolation.
Percent retainedMaterial held on a sieve, with the report defining individual or cumulative basis.Do not confuse it with percent passing.
Specified rangeAllowed limits for a result under the named requirement.Use the correct specification and edition.

For a purely illustrative reading exercise, if 70% of a sample passes a stated sieve, 30% is retained above that opening on a cumulative basis. This does not mean 70% of the individual stones were counted, and it does not establish a suitable grading for any application.

Read the curve as a whole

A broad, dense grading includes a range of coarse and finer particles. A more open grading has a different distribution with fewer particles in some smaller fractions. These descriptions explain different material structures; they are not automatic performance certifications.

Base course aggregate may be dense-graded or open-graded as the design requires. A clean fraction of crushed stone may have a different purpose even when its upper size looks similar. Match the complete distribution to the layer or mixture, not the photograph.

Check what accompanies the numbers

Look for material identification, sample or source reference, report date and the stated test method. A grading result describes the tested sample. It does not independently establish rock durability, chemical suitability, moisture condition or approval of a different source.

Local numerical names and labels such as “minus,” “clean” or a nominal size need a documented definition when the job has a specification. Do not infer a nationwide equivalent from familiar wording. Ask for clarification before comparing differently labeled products as though they are identical.

Read a sample gradation curve

Illustrative aggregate gradation curveFictional cumulative percent passing rises from 2 percent at 0.075 millimetres to 100 percent at 9.5 millimetres. At 2.36 millimetres, 70 percent passes. This is not a product grading or specification.Cumulative passing (% by mass)0204060801000.0750.150.300.601.182.364.759.5Sieve opening (mm; approximately logarithmic spacing)2.36 mm → 70% passing
Invented teaching data, not a supplied material, acceptance envelope or recommended grading. The table below gives the exact plotted values.
Sieve opening (mm)Cumulative passing by mass (%)
0.0752
0.155
0.3012
0.6025
1.1845
2.3670
4.7595
9.5100

At 2.36 mm, 70% of this fictional sample passes and 30% is cumulatively retained above that opening. Between 1.18 mm (45% passing) and 2.36 mm (70% passing), the difference is 25% of sample mass. It is not a count of individual stones.

A real review overlays or compares the complete results with the project’s specified limits at each required sieve. This curve has no acceptance limits and therefore cannot establish a pass or fail. For the test method, see ASTM C136/C136M: Sieve Analysis of Fine and Coarse Aggregates. The standard’s summary is available online; the full document is paid.

Questions buyers ask

Does nominal size mean every particle has that size?

No. A graded aggregate contains a distribution. Read the applicable definition and sieve information rather than treating the nominal label as a uniform particle dimension.

Does a passing grading prove the material meets every requirement?

No. Grading addresses size distribution. Other project requirements may concern durability, cleanliness, source composition or additional properties.

Can a photo replace a sieve report?

No. A photo helps with appearance, but it cannot measure the proportions passing each sieve or establish specification compliance.

Use gradation in your inquiry

Include the intended layer or mixture, specification name and edition, grade or class, and required sieve limits. Use the test-report guide to identify the source and sample information to request with the grading results.

When you request a quote, identify proposed alternatives separately. If you only have a local product number, include the issuing agency or the document that defines it. Ask for clarification of any missing grading before accepting an equivalent product.

Let’s start with the details.

Send the material, required grade, quantity with units and project ZIP code. Include your requested date, delivery or pickup preference and access restrictions. Mark any details that still need review.

Request quote